BÖHLER FOX 2.5 Ni伯乐焊条
Description
Ni-alloyed basic coated electrode for unalloyed and Ni-alloyed fine grained construction steels.
Tough, crack resistant weld deposit. Low temperature toughness to -80 °C.
Good weldability in all position except vertical down. Very low hydrogen content. ( according
AWS condition HD ≤ 4 ml/100 g weld metal )
Preheat 100 - 150 °C on wall thickness > 15 mm, interpass temperature max. 150 °C. Post weld
heat treatment if necessary only as required by the base metal.
Approvals and Certificates
TÜV-D (00147.), DB (10.014.16), ÜZ (10.014/1), ÖBB, ABS (Ni 2.1/2.6), BV (5Y40), WIWEB, CL
(0260), DNV (5 YH10), GL (8Y46), LR (5Y40mH15), RINA (5YH5,3H5) Statoil, UDT, SEPROZ
base Materials
cryogenic constructional steels and Ni-steels, cryogenic steels for ship building
12Ni14, 14Ni6, 10Ni14, 13MnNi6-3, P355NL1 - P460NL1, P355NL2 - P460NL2,
S255N - S460N, S355NH - S460NH, S255NL - S460NL, S255NL1 - S380NL1
ASTM A633 Gr. E; A572 Gr. 65; A203 Gr. D; A333 and A334 Gr. 3; A 350 Gr. LF3
Operating Data
re-drying if necessary: ø mm L mm amps A
300 - 350 °C, min. 2 h 2.5 350 70 - 100
electrode identifikation: 3.2 350 110 - 140
FOX 2.5 Ni 8018-C1 E 46 8 2Ni B 4.0 450 140 - 180
5.0 450 190 - 230
Preheat, interpass temperature and post weld heat treatment as required by the base metal.
Mechanical Properties of All-weld metal
(*) u s
yield strength R e N/mm 2 : 490 (≥ 460) 470 (≥ 420)
tensile strength R m N/mm 2 : 570 (550 - 680) 550 (540 - 640)
elongation A (L 0 = 5d 0 ) %: 30 (≥ 324) 30 (≥ 324)
impact work ISO-V KV J + 20 °C: 180 (≥ 110) 200 (≥ 110)
- 80 °C: 110 (≥ 347)
(*) u untreated, as-welded
s stress relieved 580 °C/2 h/furnace down to 300 °C/air
Typical Composition of All-weld metal
C Si Mn Ni
wt-% 0.04 0.3 0.8 2.4