4.根据气候变化,请远离火源,阴暗处15度-30度环境下存放
Brand: but MY name: anodic oxidation INK Numbers: 65496
Anodic oxidation ink series
The product is produced with advanced import acrylic resin and senior pigment after fine grinding system, used in combination to ABS, PP, PET, all kinds of metal, glass, ceramic, stone, electroplating (water cut electroplating), anodic alumina surface and roast (spray paint products of screen and pad printing, not needing curing agent, and does not need to bake, can obtain excellent adhesion.
Ink characteristics:
1 the classification includs glass, adhesion, good resistance to gasoline, alcohol, resistance to chemicals;
2, feel is good, flow ping **, good surface is bright and clean;
3 and fine surface hardness, impact resistance properties of strong, resistance to scratch;
4, resistant to gasoline, alcohol, resistant to chemicals resistant degree good;
Printing:
Choose for 100-350 mesh mesh to 120 T nets yarn with coverage area calculation per kilogram of 30 to 35 ㎡.
Dry time table natural volatilize 5 to 15 minutes, action in time within 24 hours, after 48 hours of optimum performance.
1. With matching special thinner, open oil and water
2. Wash washing nets with 718 net.
3. Or add hardener 10% supporting can increase adhesion, improve ink film hardness.
4. Preheat the oven to 80 ℃ bake for 10 minutes Canon even better.
Test method (dry) :
1.3 M tape stuck in the picture hass ink surface 45 degree Angle quickly pull up not to take off oil.
2. The purity of 99% alcohol 500 G force in ink surface wipe 300 times back and forth without decoloring.
Method of use:
1. The proposal with my company special thinner to dilute, not recommended dry thinners diluted 783 slow, before the use should be fully mixing, use at any time after sealing.
2. Add the company supporting stirring open 10 to 12%, oil and water dilute the printing for viscosity, pad printing dilution use moving printing special thinner,; Use clean water to wash the nets 718.
3. Not with other kinds of printing ink mixed use, otherwise easy to have other adhesion, chemical reactions and other bad phenomenon.
4. Add hardener inks use time limit for 8 hours, please not used, the remaining expired ink not recycling
Note:
1. All kinds of printing material appearance similar, but may be of different material, customers are required to meet the requirements of the ShiYin, indeed, its, then batch production.
2. In moving printing process, such as a wire drawing or away, can be appropriately to add some slow dry paste can;
3. Environmental temperature is too high, will influence the quality of the original ink. White will change color, roasted beyond 150 when please use woodiness material bottom, and may not directly contact roast iron
4. According to climate change, please away from fire, the shadows 15 degrees-30 degrees environment for